Melting Point: 110–115 ℃ (DSC) Density: 1.35–1.45 g/cm³ Hardness: 85–90 (Shore) Linear Expansion: 0.01% Thermal Decomposition Residue: <1.0% Antistatic: Yes Composition: PMMA >99%, pigment <0.1% Organic Residues: <1.0% Application: Milling of temporary restorations Processing Parameters: Spindle Speed: 18,000 – 20,000 rpm Rough Milling: 0.5 mm Fine Milling: 0.05 mm